Silicon Barium Alloy Silver-gray

Silicon Barium Alloy Silver-gray

Silicon-Barium, also known as barium-silicon modifier, is a long-term graphitization. Compared with ferrosilicon, it is able to increase the thickness of the cross-sectional structure and the uniformity of hardness
Anfrage senden
Beschreibung
Technische Parameter
silicon barium alloy silver-gray Description

 

Silicon-barium alloy is a combination of silicon, barium, and iron. This alloy is an ideal deoxidizer and desulfurizer for smelting high-quality steel. Silicon-barium alloy is usually smelted in an electric furnace, which requires significant energy consumption. An alternative method is to produce in an intermediate frequency furnace. The main production is located in the north-western region. China's silicon-barium alloy exports mainly go to countries in the Asia-Pacific region, including Japan, Australia, and some European and American countries.

 

Calcium Silicon Barium Silver-Gray Alloy Manufacturers

Calcium Silicon Barium Silver-Gray Alloy Manufacturers

 

 

 

The Specification Of silicon barium alloy silver-gray

 

 

 

Si-Ba Inoculant

 

Ba3 Si65

0.5-2.0

60-65

2-4

0.5-2.5

Ba5 Si60

2-5

55-60

4-6

0.5-2.5

Ba10 Si55

0.2-3

50-55

8-12

3.5-5.5

2-8

Ba15 Si50

0.2-3

45-50

13-17

3.5-5.5

2-8

Ba20 Si45

0.2-3

40-45

18-20

3.5-5.5

2-8

Ba3 Si50

0.2-3

46-54

1.5-4

1-3

2-8

 

 

 

 

 

 

Calcium Barium Silicon Alloy Silver-Gray Suppliers

Calcium Barium Silicon Alloy Silver-Gray Suppliers

 

 

 

 

 

 

 

Barium Silicon Calcium Alloy Silver-Gray For Sale

Barium Silicon Calcium Alloy Silver-Gray For Sale

 

 

 

 

 

 

 

 

 